1074/1075 Scaleless Tempered Spring Steel is comprised of medium-high carbon which makes for better forming qualities than 1095 blue tempered. This Blue Tempered Spring Steel retains good forming properties. Typically used where the higher carbon content is not needed.
Unit of Measure
Thickness |
N/A 0.042 in1.0668 mm |
Width |
N/A 24 in609.60 mm |
Length |
N/A 48 in4.00 ft1219.20 mm |
Grade/Alloy |
N/A 1075 |
Shape |
N/A Flat Sheet |
Size |
N/A 24 x 48 in |
Material |
N/A Blue Temper |
ASTM |
N/A A 684 |
Market Applications |
N/A Clips Coiled and Flat Mechanical Springs Steel Tapes Washers |
Temper Rating |
N/A Hardened and Tempered |
Hardness |
N/A RC 44/47 (ref. only) |
Specifications |
N/A AMS 5122 per Chem. ASTM A 684 MIL-S-7947 per Chem. |
Tensile Strength |
N/A NA |
Yield Strength |
N/A NA |
Elongation (% in 2 in.) |
N/A NA |
Surface Finish |
N/A Blue Polished |
RA (um) |
N/A 15 RMS max. |
Grain Size (RTF in mm) |
N/A NA |
RoHS |
N/A RoHS Compliant |
REACH |
N/A REACH Compliant |
DFARS |
N/A DFARS Compliant Upon Request |
Country of Manufacture |
N/A USA |
C |
N/A 0.69 to 0.80 |
Mn |
N/A 0.40 to 0.80 |
Fe |
N/A 98.38 to 98.8 |
P |
N/A 0.02 max |
S |
N/A 0.025 max |
Si |
N/A 0.15 to 0.30 |
0.025 |
N/A ±0.001 |
0.032 |
N/A ±0.0015 |
0.035 |
N/A ±0.002 |
0.042 |
N/A ±0.002 |
0.050 |
N/A ±0.002 |
0.062 |
N/A ±0.002 |